A 5G patch on an ultra-low-permittivity ceramic, checked against the textbook formulas

A 2025 paper makes a Ca3(BO3)2 microwave ceramic with εr 5.95 and simulates a 14.97 GHz patch antenna on it. The transmission-line model reproduces its width to within 0.5 % and explains the length.

Microwave ceramics are usually sold on a high dielectric constant, because a high εr shrinks the circuit. For an antenna the trade runs the other way: a low εr keeps more of the field in the air, which is where the radiation has to come from. A 2025 paper in Crystals makes a calcium borate, Ca₃(BO₃)₂, with an ultra-low εr of 5.95 and a good quality factor, then simulates a 14.97 GHz microstrip patch on it, reporting a footprint of 3.75 × 5.4 × 1.4 mm and 7.15 dBi of gain. A patch is one of the few antennas whose size follows from closed-form formulas, so the claim can be checked on a phone with the antenna calculator. For what to do with the feed afterwards, see the smith chart; for the ceramic’s other life as a waveguide filler, see waveguide mode calculator.

The paper in brief

The authors sintered Ca₃(BO₃)₂ (CBO) under 800 MPa and measured its microwave properties: εr = 5.95, a quality factor Q × f = 11,836 GHz, and a temperature coefficient of resonant frequency τf = −39.89 ppm/°C. An εr near 6 is low for a dense ceramic; most microwave ceramics sit between 20 and 40, and only polymers and foams go much lower.

They then simulated a rectangular microstrip patch on a 1.4 mm board of the material, quoting dimensions of 3.75 × 5.4 × 1.4 mm, a resonance at 14.97 GHz, a return loss of −25.5 dB and a peak gain of 7.15 dBi broadside. The argument is that a low-εr, low-loss ceramic is the right substrate for millimetre-wave 5G patches.

Checked with the tools

Everything here is a recomputation from the paper’s stated permittivity, thickness and frequency with the transmission-line model, the standard closed form for a rectangular patch. We do not re-run their electromagnetic simulation. Our reading of the quoted dimensions is that 5.4 mm is the patch width, 3.75 mm the resonant length and 1.4 mm the substrate thickness; no other arrangement gives a patch anywhere near 15 GHz on this ceramic.

Step 1: the width lands almost exactly. For good radiation efficiency the model takes W = c/(2f)·√(2/(εr + 1)). At 14.97 GHz with εr 5.95 that is 5.371 mm, against the paper’s 5.4 mm: 0.5 % apart. Read the other way, a 5.4 mm width is the textbook width for 14.89 GHz. The paper’s board was clearly sized with this formula, or something equivalent to it.

Step 2: the length is 7 % longer than the thin-substrate formula wants. The model’s resonant length is L = c/(2f√εeff) − 2ΔL, with an effective permittivity of 4.693 (part of the field runs in the air above the board) and a fringing extension ΔL of 0.574 mm at each radiating edge. That gives 3.473 mm, while the paper has 3.75 mm, 7.4 % longer. Turned around, the model says a 3.75 mm patch on this ceramic resonates at 14.06 GHz, about 6 % below the simulated 14.97 GHz.

Which frequency fits a 3.75 mm length?Which frequency fits a 3.75 mm length?34512131415161718Frequency (GHz)Design length L (mm)the paper's 3.75 mm14.06 GHz (model)14.97 GHz (paper)fibub.com
Figure 2. The same model read backwards: the design length falls as frequency rises, and the paper's 3.75 mm length is resonant at 14.06 GHz in the model against the 14.97 GHz of its full-wave simulation.

That gap is expected, and it is worth knowing which way it goes. The substrate here is 1.4 mm on a 20.03 mm free-space wavelength: h = 0.070 λ₀, and h = 0.15 λg inside the dielectric. The transmission-line model with Hammerstad’s fringing is a thin-substrate approximation; above roughly h = 0.05 λ₀ it underestimates the fringing fields, so it asks for a shorter patch than a full-wave simulation does. fibub’s tool refuses the calculation altogether above h = λ/10 (2.00 mm here), which is a reminder rather than a guarantee: at 0.07 λ₀ you are already in the band where a few per cent of error is normal. Anyone designing on this ceramic should take the closed form as a starting point and expect to tune down by a few per cent, which is exactly the difference the paper’s own numbers show.

Step 3: what the low permittivity is actually buying. The tool makes the trade-off concrete. At the same 14.97 GHz and 1.4 mm thickness, the patch area is 18.7 mm² on this εr 5.95 ceramic, but only 3.97 mm² on a conventional εr 25 microwave ceramic: the high-εr board is 4.7 times smaller. The low-εr patch pays for its size with a much lower effective permittivity (4.69 against 17.5), which means more of the field in the air, and with a far friendlier feed: the edge resistance is 369 Ω here against 1,209 Ω at εr 25, so the inset feed that matches 50 Ω needs a notch 1.32 mm deep rather than a much deeper and lossier one. Those are the mechanisms behind the paper’s headline claim, in numbers a reader can reproduce.

Patch size at 14.97 GHz against substrate permittivityPatch size at 14.97 GHz against substrate permittivity02468510152025Substrate relative permittivity εrPatch dimension (mm)the paper's ceramic, εr 5.95Width WLength LPaper's footprintfibub.com
Figure 1. Patch width and length at 14.97 GHz on a 1.4 mm substrate, worked out with the Antenna calculator's transmission-line model, as the substrate permittivity changes. The two black dots are the paper's own footprint at its ceramic's εr of 5.95.
Check Paper Tool (transmission-line model)
Patch width at 14.97 GHz 5.4 mm 5.371 mm (0.5 % apart)
Patch length at 14.97 GHz 3.75 mm 3.473 mm (7.4 % shorter)
Resonance of a 3.75 mm patch 14.97 GHz (simulated) 14.06 GHz
Effective permittivity not stated 4.693
Edge resistance, inset depth for 50 Ω not stated 369.3 Ω, 1.32 mm
Ground plane (patch + 6h) not stated 13.77 × 11.87 mm
Substrate thickness in wavelengths not stated 0.070 λ₀, 0.15 λg

How we made the graphs

The charts and every number come from scripts/blog-figures/low-permittivity-ceramic-patch-antenna-transmission-line-model.mjs in fibub’s public code. It calls patch() from src/lib/sci/eng-antenna.ts, the maths behind the antenna calculator: the width formula, Hammerstad’s effective permittivity and fringing extension, the resonant length, the radiating-slot conductance G1 and mutual conductance G12 (both numerical integrals, with a Bessel J₀ inside G12), the edge resistance and the inset depth that matches a 50 Ω line. The frequency that fits a given dimension is found by bisection on the tool’s own output.

From the paper: εr 5.95, the 1.4 mm thickness, the 14.97 GHz resonance and the 3.75 × 5.4 mm footprint. Our own choices: reading those dimensions as length × width, the εr 2.2 to 25 range in Figure 1, and the 50 Ω feed.

How we test the maths

On every change to fibub, tests/sci.mjs runs tests/sci-tools/antenna-calculator.mjs, which pins this maths against Balanis’s worked examples and an independent SciPy implementation:

  • Balanis’s design example, a patch at 10 GHz on εr 2.2 and h 0.1588 cm, must come back as W = 1.186 cm, εeff = 1.972 and L = 0.906 cm, the book’s own numbers.
  • The radiating-slot conductance and the inset depth must match SciPy’s numerical integration of the same integrals, and the Bessel function J₀ must match scipy.special.j0.
  • New with this article: the paper’s ceramic, 14.97 GHz with εr 5.95 and h 1.4 mm, must give W = 5.3714 mm, L = 3.4734 mm, εeff = 4.6932, ΔL = 0.57430 mm, an edge resistance of 369.33 Ω and a 50 Ω inset depth of 1.3201 mm.

Check it yourself

On the antenna calculator page:

  1. Press Patch in the antenna-type row. The frequency unit switches itself to GHz.
  2. Frequency 14.97, Substrate relative permittivity εr 5.95, Substrate thickness h (mm) 1.4, Feed line impedance for the inset (Ω) 50.
  3. The headline reads Patch 5.371 mm wide × 3.473 mm long. In the facts below: Effective permittivity εeff 4.693, Fringing extension ΔL 0.5743 mm, Edge resistance 369.3 Ω, Inset depth for 50 Ω 1.32 mm, Ground plane at least 13.77 mm × 11.87 mm.
  4. Change Frequency to 14.06 and the length becomes 3.75 mm, the paper’s own dimension.
  5. Put Substrate relative permittivity εr up to 25, a normal microwave ceramic, and watch the patch fall to 2.777 × 1.431 mm while the edge resistance climbs to 1209 Ω: smaller, but much harder to feed and with less of its field in the air.
  6. Type Substrate thickness h (mm) 2.5 and the tool refuses the calculation: above λ/10 (2.003 mm at this frequency) the model is no longer a fair approximation.

What researchers can use it for

  • Sanity-check a published patch in a minute: type the stated εr, thickness and frequency and see whether the quoted footprint is the textbook one, as we did here.
  • Report what the closed form predicts alongside a full-wave simulation, so readers can see how much of the final size came from tuning.
  • Choose a substrate for a new ceramic: sweep εr and watch the patch area, the effective permittivity and the edge resistance move together, instead of arguing about size alone.
  • Plan the feed before the board: the edge resistance and inset depth say whether a 50 Ω line can be matched directly or needs a quarter-wave section, which the smith chart then handles.
  • Teach the limits of a model: the h/λ ratio and the refusal above λ/10 make the approximation’s boundary visible, which is hard to show with a simulator.

The fine print

  • The paper gives one combined dimension string (3.75 × 5.4 × 1.4 mm) and does not label which number is which, nor the feed type or position. Our reading is stated above; if the 3.75 mm is something else, the length comparison changes.
  • The transmission-line model gives sizes, not gain or return loss. The paper’s 7.15 dBi and −25.5 dB cannot be checked this way; a 7 dBi broadside gain is, however, in the normal range for a single patch on a thick, low-εr substrate.
  • We used the paper’s εr at its working frequency as stated. Permittivity drifts with frequency and temperature (the paper’s own τf is −39.89 ppm/°C), which moves the resonance by far more than our 0.5 % width agreement suggests is achievable in a real board.
  • Nothing here is a measurement of the ceramic. The dielectric data are the paper’s.

Sources

  • Liu, F., Song, F., Zhu, W., Zhang, Z., Yao, Z., Liu, H., Sun, H., Lin, G., Xu, Y., Zhang, L. et al. (2025), Ultra-Low Dielectric Constant Ca3(BO3)2 Microwave Ceramics and Their Performance Simulation in 5G Microstrip Patch Antennas, Crystals 15(7): 599, doi:10.3390/cryst15070599. Licence CC BY 4.0, checked on the MDPI article page and in the Crossref record, 2026-11-24; no correction or retraction is recorded. Values used here: relative permittivity 5.95 for the ceramic sintered under 800 MPa; Q x f = 11,836 GHz; temperature coefficient of resonant frequency -39.89 ppm/C; simulated antenna dimensions 3.75 x 5.4 x 1.4 mm; resonance 14.97 GHz; S11 -25.5 dB; peak gain 7.15 dBi at theta = 0.
  • Transmission-line model of a rectangular microstrip patch, with Hammerstad's fringing extension, the radiating-slot and mutual conductances and the inset feed: Balanis, C. A., Antenna Theory: Analysis and Design, chapter 14. Speed of light: the exact SI value.

If you are an author or publisher and want a credit or a passage changed or removed, tell us and we will act quickly.